fakhfakh
Industrial
- Nov 11, 2004
- 48
Dear All,
Ou client requires to perform heat treatment after the manufacturing of a pressure vessel to ASME VIII Div 1
Mtrl: SA 240 310S
Thick: 26 to 28mm
Welded
The Code do not require neither prohibit a PWHT
Normally such type of mterial needs a heat treatment to a temperature 1050-1100°C
Is it necessary to perform fast cooling after heating knowing that it is almoste impracticable?
Thank you
Ou client requires to perform heat treatment after the manufacturing of a pressure vessel to ASME VIII Div 1
Mtrl: SA 240 310S
Thick: 26 to 28mm
Welded
The Code do not require neither prohibit a PWHT
Normally such type of mterial needs a heat treatment to a temperature 1050-1100°C
Is it necessary to perform fast cooling after heating knowing that it is almoste impracticable?
Thank you