I'm currently using grade AC2B Al alloy to cast break master and clutch master, using gravity die mould. In what way can i enhance the properties of this material..? Like in alternative HT..
The AC2B aluminum alloy designation is listed under Japanese Casting specification KSD 6008. A cross reference with this casting specification indicates the AC2B is an AA 319 Aluminum alloy casting - F or T6.
The AA 319 can be sand cast or permanent mold cast. There are three strength levels based on tempers offered by some foundries;
AA 319 -F as cast, lowest strength ~ 27 ksi min UTS