Hi all,
I'm facing this problem, can anyone help?
Required specs....
material: JIS SNCM220 (AISI 8620)
carburised to achieve:
surface hardness 600~700 HV
EHT 550 HV at 0.3~0.5mm
core hardness 390~450 HV
Obtained hadness readngs....
at 0.05mm : 646 HV
at 0.1mm : 585 HV
at 0.2mm : 470 HV
at 0.3mm : 384 HV
at 0.5mm : 336 HV
at 0.6mm : 298 HV
at core : 426 HV
I can tell that the case depth is out of specs, and that the core hardness is reasonably good, but I do not understand why it's so "soft" at the depth of 0.3~0.6mm.
Thank you.
Best regards,
ct
I'm facing this problem, can anyone help?
Required specs....
material: JIS SNCM220 (AISI 8620)
carburised to achieve:
surface hardness 600~700 HV
EHT 550 HV at 0.3~0.5mm
core hardness 390~450 HV
Obtained hadness readngs....
at 0.05mm : 646 HV
at 0.1mm : 585 HV
at 0.2mm : 470 HV
at 0.3mm : 384 HV
at 0.5mm : 336 HV
at 0.6mm : 298 HV
at core : 426 HV
I can tell that the case depth is out of specs, and that the core hardness is reasonably good, but I do not understand why it's so "soft" at the depth of 0.3~0.6mm.
Thank you.
Best regards,
ct