"actually pure iron holds strength better than most alloys. We used to build retorts for sintering furnaces out of 1002, and they ran at 2350F (1288C)"
Ed, you are right ,for salt bath electrodes, low carbon steel (< 0.1%), would perform better than 35/15 (Grade HT).
"Even,if you are a minority of one, truth is the truth."