PJBurr
Industrial
- Nov 18, 2003
- 2
I’m interested in using 6160T-6 aluminum for machined components in a location devise. My concern is long-term wear. I understand heat-treating is an option. I am not too familiar with non-ferrous heat-treating.
What wear properties can I expect to achieve through heat-treating? With component dimensions of approximately 0.75”x6.0”x12.0,” what range / scale would allow increase wear without creating a brittle plate?
Any assistance or links to assistance is appreciated.
What wear properties can I expect to achieve through heat-treating? With component dimensions of approximately 0.75”x6.0”x12.0,” what range / scale would allow increase wear without creating a brittle plate?