I have two different plates of 4130, both heat treated to a hardness of HRC 22, the but it looks like both plates are heat treated differently as the color of the finished plates is different. Plate sample A is a dark gray to black while plate sample B is a light gray.

Is the finished color a result of the quench media? For example one plate could be quenched with oil and the other water or brine?

Initially I though the tempering would effect the color, but given that they both have the same hardness value this maybe not the case.
 
Replies continue below

Recommended for you

The finished color can depend upon several factors. The type of quenchant can affect the final color. In this particular case, I would speculate that the dark color is darkened/decomposed quenchant and/or scale from tempering. The light gray color likely is the base metal color due to a descaling/cleaning operation after the tempering process.
 
Could it be that part was heat treated in a vacuum rather than atmosphere? Would this have any effect on the color?

 
Furnace atmosphere can play a large role in material surface color.
 