We have a 17/7 PH rather complex structure of 0.050" 1.5" diameter tubes that is being welded together with 17/7 filler. To get the full strength after weld we plan on solution treating at 1900 Deg F, and then Austenitize at 1400 Deg F and then Harden at 1050 Deg F (TH1050). The structure is 15 ft long, so we will be heat treating in air and want to inhibit heat treat scale growth. Our research found a product ATP 641 for coating stainless steel that we are considering. Does anyone have any experience with this product or can anyone suggest another product. The following is a link to the ATP 631.


Kim R. Taylor PE
Mechanical Engineer
 
Anneal in hydrogen, Austenite condition in either hydrogen or vacuum, and then age in vacuum.
At worst you will end up with a light heat tint

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 