Just looking for any information on heat treating the above steel.
Through hardening procedures, & carburizing (case depth .008-.012) core hardness ? if final case hardness at 58 min.
plus any data on mar quenching or mar tempering if it's possible.
Thank You
Through hardening procedures, & carburizing (case depth .008-.012) core hardness ? if final case hardness at 58 min.