We are placing three electrical components in close proximity to one another and it has been determined that there must be a heat sink/heat spreader plate to keep the temperature within operating range. What would you suggest as a material to use for this heat spreader plate. I've heard aluminum 6061 and 6063 suggested.
 
Replies continue below

Recommended for you

Or if possible, just redesign it to put these parts in direct contact with the chassis..avoid the need for a spreader at all.
 