The following heat number / identification markings were taken off some steel plate. Can anyone help me identify it?

75A679 287993 AAR-TC 128GRB USS

I recognize the material - AAR-TC128 GRB.
I think the Mill is US Steel
I'm not sure of the meaning of the digits of the first two number groupings.

Thanks
 
Replies continue below

Recommended for you

rbrez,
Do you have a material test report by any chance? I believe you have correctly identified the mill. It is possible that the first two number groupings constitute the heat number although it is possible that the 75A679 is a reference to the 1975 edition of ASTM specification A679 for high tensile, cold drawn steel wire, although I see no reason this would appear on plate. Are these the original mill markings? Where did you procure this material from and what is the intended fabrication/service?
Regards,
RLS
 
Thanks for the reply. That is the problem, I do not have the Mill test reports. I agree that the 75 could be the year. The plate TC 128 GRB is a special plate used in the railcar tank building industry. I am just trying to find out what the code markings mean.
 