Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Heat measuring sensors 1

Status
Not open for further replies.

p1vrg

Mechanical
Joined
Jan 13, 2004
Messages
5
Location
GB
Hi,
I would like to know if anyone can tell me what type of senor could i use to measure the temperature change in a tensile test piece made of aluminium. The tensile tester is the Lloyds LS series. The test pieces measures 60mmx30mmx3mm. The change in temperature must be measured to within 0.1 degree.

Thanks
 
If you need to measure during the tensile test, it is not so
simple: you must assure good termal coupling without coupling the stress into the sensor. Most likely you can
satisfy both requirements only partially and this will make it necessary to slow down the test.


<nbucska@pcperipherals.com>
 
Perhaps an IR non-contact thermometer will do the job, depending on the temperaure change you would like to measure. The resolution is about 0,1 deg C.