Heat Insulation Material

Status
Not open for further replies.

Speedy

Mechanical
Joined
Jun 5, 2001
Messages
229
Location
DE
We currently have an application that requires 'spacers' to heat insulate 2 plates of aluminium. One plate is at 170C, the other at 60C. The spacers are cylindrical in shape and are highly stressed (don't know the exact load as it is a clamping arrangement).

The company doing the design work believe that there is no insulation material available that combines the properties of high insulation, machinability and high dimensional stability / strength under load.

Does anybody know of materials we could look at?
Speedy

"Tell a man there are 300 billion stars in the universe and he'll believe you. Tell him a bench has wet paint on it and he'll have to touch to be sure."
 
What's wrong about Aluminium Oxide (exept for the expense)? It is available in rods and tubes and is quite strong.

The temperature-differance is small I think, why not use insulating spacers? I have made spacers from a sheet of mica with a hole-punch myself and it worked fine for me with a temparature up to 800C!

Maybe you can give more details, the clamping-load on the spacers, the distance between the plates. Simple RVS has a rather low heat-conduction, so that might help?

Regards,

Pekelder
 
Status