Good morning,
As the title suggests is there a general consensus on whether or not Thermal Efficiency (E) being factored into the heat input equation produces a more accurate joules reading? If so why has ASME/AWS not adopted this into their equations as of yet? Please see below.
Typical ASME/AWS - (V)x(I)x(60)/Travel Speed
EN 1011-1 - (V)x(I)x(60)x(E)/Travel Speed
Thank you
Allan James
As the title suggests is there a general consensus on whether or not Thermal Efficiency (E) being factored into the heat input equation produces a more accurate joules reading? If so why has ASME/AWS not adopted this into their equations as of yet? Please see below.
Typical ASME/AWS - (V)x(I)x(60)/Travel Speed
EN 1011-1 - (V)x(I)x(60)x(E)/Travel Speed
Thank you
Allan James