thread391-130156
Any design input for making a heat exchanger to regulate the discharge temperature of compressed nitrogen gas for flightline use (i.e. service struts & tires). HX to be sized so that discharge temperature is -60F or warmer with constant supply of nitrogen at flow rates up to 32 SCFM. Fan supplied with HX shall be driven by a motor that operates from compressed nitrogen as well.
 
I'm assuming that you are a new member, so welcome. Note that the cited thread is 8 years old.

you may wish to change the display order of threads to "by date" in "My Profile"

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529
 
Al is commonly used for pure gas HX applications.
If your pressures are too high for reasonable wall thickness then move to SS.


= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 