I have done about 5 coupons/tests on this procedure and cannot seem to get the HAZ hardness better than 5-10 too hard in Vickers (255-260).
We are using pulsed TIG machines.
0.2/0.2 high/low
50% background current
~270 amps
0.9 inch Z step per revolution
400-500F preheat
7-10 IPM travel speed *table*
~80 IPM wire feed speed
After welded we wrap it up and cool down.
Does anyone have an idea of where to go from here? We are conforming to NACE/API/ASME.
We are using pulsed TIG machines.
0.2/0.2 high/low
50% background current
~270 amps
0.9 inch Z step per revolution
400-500F preheat
7-10 IPM travel speed *table*
~80 IPM wire feed speed
After welded we wrap it up and cool down.
Does anyone have an idea of where to go from here? We are conforming to NACE/API/ASME.