Hi all,
Any idea on why the hardness values for the SA335 304H, SA312 304H and SA403M WP304H stainless steel and most of the stainless steels are not mentioned in the specification? The hardness for stainless steel is only specified in SA231 tubes. Can we take minimum tensile strength in stainless steel and convert them to hardness as the reference minimum hardness? or can we use the hardness values in SA213 as a reference for any other class of stainless steel?
Comments are welcome....
Happy New Year to all...
Any idea on why the hardness values for the SA335 304H, SA312 304H and SA403M WP304H stainless steel and most of the stainless steels are not mentioned in the specification? The hardness for stainless steel is only specified in SA231 tubes. Can we take minimum tensile strength in stainless steel and convert them to hardness as the reference minimum hardness? or can we use the hardness values in SA213 as a reference for any other class of stainless steel?
Comments are welcome....
Happy New Year to all...