We have a OEM part casted with IC 8620, hardness requirement is annealed Rockwell 82~90 Rb.
The problem encounted is :
Shall we remove the scale (or decarburization) before testing the hardness on a casted part ?
We tested the hardness on a flat surface and the hardness reading seems unstable, some of them < 80 Rb and some of them > 90 Rb. But the heat treater tested it on the ground gate area with all data within the specified range. The heat treater insists that's the right place to test the hardness since the gate already ground. Why we have to test it on the ground area ? Any one who can give me the reasons.
Thanks in advance for any inputs.
The problem encounted is :
Shall we remove the scale (or decarburization) before testing the hardness on a casted part ?
We tested the hardness on a flat surface and the hardness reading seems unstable, some of them < 80 Rb and some of them > 90 Rb. But the heat treater tested it on the ground gate area with all data within the specified range. The heat treater insists that's the right place to test the hardness since the gate already ground. Why we have to test it on the ground area ? Any one who can give me the reasons.
Thanks in advance for any inputs.