Dec 15, 2016 #1 shonuff Industrial Joined Aug 15, 2013 Messages 20 Location US Had some scaffold boards that got hot enough during PWHT to smolder and possibly have an open flame. Boards were put out buy water hose. If I were to do hardness test on this pipe is there a specific way or layout of the test on the pipe?
Had some scaffold boards that got hot enough during PWHT to smolder and possibly have an open flame. Boards were put out buy water hose. If I were to do hardness test on this pipe is there a specific way or layout of the test on the pipe?
Dec 15, 2016 #2 hsemus Petroleum Joined Apr 26, 2012 Messages 42 Location GB try to use a grid with a spacing 25mm for each hardness measurement . This hardness test can be performed by a portable hardness reader. Upvote 0 Downvote
try to use a grid with a spacing 25mm for each hardness measurement . This hardness test can be performed by a portable hardness reader.