Dear All,
I am a mechanical engineer and have problem understanding something related to metallurgy so please help me.
Is there a mechanism based on which a carbon steel becomes harder and harder as time goes by?
I mean suppose that I have a steel with yield stress 250 MPa and I put it aside in a warehouse which is a place with normal temperature and after two years I have the same steel which has a higher strength like 260 MPa? Is it possible and what could be the cause of it?
Warm Regards
I am a mechanical engineer and have problem understanding something related to metallurgy so please help me.
Is there a mechanism based on which a carbon steel becomes harder and harder as time goes by?
I mean suppose that I have a steel with yield stress 250 MPa and I put it aside in a warehouse which is a place with normal temperature and after two years I have the same steel which has a higher strength like 260 MPa? Is it possible and what could be the cause of it?
Warm Regards