I am trying to do an elasto-plastic analysis in Mechanica. What is a good source to obtain either the data or equation of hardening law for some metals such as 17-4PH, Al 7075-T6 etc

Thanks
YSM
 
Physical testing or atlas of stress strain curves.

Remember, to convert the engineering stress strain data to true stress vs plastic strain data.

Steve


Stephen Seymour, PE
Seymour Engineering & Consulting Group
 
Thanks Steve, I will see if I can get access to the Atlas and check it out. Thanks again

YSM
 
Steve,
I got hold of the book. I have attached the graph for heat treat H925.
Can I use the graph (attached) as it is in Mechanica or do I have to convert the beyond-yield part of the curve for hardening using the Ramberg-Osgood parameters. If so only the n value is given, how can i obtain either the K in the formula

Strain = (Sigma/E) + K(Sigma/E)^n

or alpha in the formula

Strain = (Sigma/E) + alpha*(Yield/E)*(Sigma/Yield)^n

Thanks for your help.
ysm

 
 http://files.engineering.com/getfile.aspx?folder=e279f15e-33b9-470f-8a8b-3576de0a6d66&file=15-5PH.jpg