I am modeling a compression test of fresh concrete (1 hour age) by ABAQUS CAE. According to literature the best plasticity model for such material is Mohr-coulomb model.
I have the following material properties.
Material density ϒ = 2.07 e-9 tonnage/mm3
The Young's modulus E= 0.154 Mpa
Poisson ratio v =0.3
Cohesion C =0.0065 Mpa
Angle of internal friction φ = 20
Dilation angle Ψ = 13
the aim of this simulation to validate stress strain curve of the experiment. Unfortunately the stress-strain curve I obtained is totally different.
I attached my input and resulted curve with that of real experiment.
Any one can help in this regard ?
I am modeling a compression test of fresh concrete (1 hour age) by ABAQUS CAE. According to literature the best plasticity model for such material is Mohr-coulomb model.
I have the following material properties.
Material density ϒ = 2.07 e-9 tonnage/mm3
The Young's modulus E= 0.154 Mpa
Poisson ratio v =0.3
Cohesion C =0.0065 Mpa
Angle of internal friction φ = 20
Dilation angle Ψ = 13
the aim of this simulation to validate stress strain curve of the experiment. Unfortunately the stress-strain curve I obtained is totally different.
I attached my input and resulted curve with that of real experiment.