I need some wisdom.
I have a part that is 17-4 H900 stainless steal that was hard chrome coated, and electro-polished. The problem is that they coated my threads too. I have removed the chrome from the threads but I am trying to determine if there is residual degradation of my part fatigue life from the chroming?
The threads were not supposed to be coated, they screwed up! The company that did it states that there is no residual effects... but I know chroming can decrease endurance by as much as 50%. Did the chrome removal restore my endurance? If not how much did it decrease (%)?
Thanks
I have a part that is 17-4 H900 stainless steal that was hard chrome coated, and electro-polished. The problem is that they coated my threads too. I have removed the chrome from the threads but I am trying to determine if there is residual degradation of my part fatigue life from the chroming?
The threads were not supposed to be coated, they screwed up! The company that did it states that there is no residual effects... but I know chroming can decrease endurance by as much as 50%. Did the chrome removal restore my endurance? If not how much did it decrease (%)?
Thanks