We are a retailer of Prestressed Concrete Strands 9.5mm (ASTM A416). Our customer experienced slippage on their Precast Half Slab and bonding problem with concrete due to oiled Strands. Our supplier informed us that they applied Water-Soluble Oil and it will be dried by natural air drying for 2-3days. After several days out in the open-air, there is still oil/grease residue on the strands as seen in attached image and our customer has lost confidence of using the remaining stocks of strands which is 88 metric tons (16 coils).
I would like to receive your insights and solution on how to remove the oil, what type of chemical to apply to it and speed up the process to remove it totally to salvage the remaining affected stocks of strands.