I am looking for are replacement level instrument for 96-98% H2SO4 in a tank with high turn-over and water addition. The current air bubblers (used for indication) tend to fail regularly due to the tubes blocking with corrosion products. THe new isntruments are part of a control system and therefor need higher reliability.
There has been considerable corrosion of dip legs in this tank, as well as of the mild steel roof. Acid spray and mist levels are high, and the surface is not even.
Thanks
I am looking for are replacement level instrument for 96-98% H2SO4 in a tank with high turn-over and water addition. The current air bubblers (used for indication) tend to fail regularly due to the tubes blocking with corrosion products. THe new isntruments are part of a control system and therefor need higher reliability.