H2 Embrittlement of ASTM 4140/4142 after cad plating? 2

Status
Not open for further replies.

jasgeer

Materials
Joined
Feb 22, 2002
Messages
7
Location
US
After cad plating stainless steels we normally specify a baking procedure to avoid hydrogen embrittlement issues. Do high strength steel materials like 4037/4140/4142/8637/8740 that are cad plated have problems with hydrogen and also need baking?
Thank you for your assistance,
Jim
 
You must ABSOLUTELY specify hydrogen embrittlement relief for quenched & tempered, martensitic steels like 4037/4140/4142/8637/8740. ASTM B 849, SAE/USCAR-5, and SAE AMS 2759/9 are all suitable standards to reference for the requirements of time and temperature depending on the strength/hardness of the parts.
 
The plating specification details baking requirements.
Go to Enter QQ-P-416 for Document ID
Download QQ-P-416F PLATING, CADMIUM (ELECTRODEPOSITED).
Use your browser back arrow and also download Amendments 2 and 3.
 
We are a spare parts manufacturing facility in the Philippines.At present we are developing a product which requires corrosion tests like
1)plating thickness,2)corrosion resistance,3)embrittlement and 4)plating adhesion test.The tests should be conducted by an external facility.We were able to have the first two tests performed at a government testing facility.However,we are having problems with the other two(embrittlemnt and plating adhesion)since we cannot find a facilty here in the Phils. who will perform such tests.
Can I have an info on external facilities who conduct such tests for other companies?Preferrably,the facility is located within Southeast Asia.
thank you very much.
 