I have an existing mezzanine that I need to evaluate the capacity of. The mezzanine uses what looks like prefabricated gypsum panels that are supported by open-web steel joists. The panels are approximately 2" think and span 3'-6" +/- (steel joist spacing).

Does anyone have any information on these panels and their load capacities?

IMG_7681_vhzrhk.jpg

view from underside

IMG_2757_cweu7h.jpg

view from top of mezzanine

IMG_2758_qls4oe.jpg

cross section view of panels
 
I ran into these same panels for the first time as well maybe two weeks ago. Mine were used for roof framing.
There is a similar product apparently still available by Martin Fireproofing. They have load tables (attached)
The Gypsum ones were possibly by a company called US Gypsum. I did not have luck finding load tables on-line. (2015 article attached)they mention a US gypsum specification guide 1971.
Photo_a_toxgxj.jpg
Photo_b_iw4d5g.jpg



 
Those look like a Bulb-T system.


Not sure they were ever approved as flooring, they are a bit low capacity and don't feel very ductile to me, then again, neither does Tectum. I know at one point I found some information on them, including some diaphragm testing? These are more of a roof plank system to me.

A few links -



Diaphragm strength:
 