Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Gunite Pool Repair

Status
Not open for further replies.

ChamboEng

Structural
Apr 26, 2016
2
Client needs to replace a pipe within a gunite pool. He's concerned that during the removal of the existing pipe, mostly likely by chiseling, he's going cause damage to the surrounding gunite. Even though gunite is a cementitious material, I don't think that it will hold up similar like concrete would...

Are there certain repair techniques that need to be implemented to mitigate additional damage to the gunite shell?

Thanks.
 
Replies continue below

Recommended for you

Maybe use a smaller percussion chipping hammer like an electric 10-lb'er?

Gunite (pneumatically applied concrete = shotcrete) is usually pretty dense stuff if applied correctly, so the usual concrete repair 'rules' would apply, IMO.
 
I'd core a hole with a diamond bit core barrel. The annuylar space later can be caulked.
 
Agree with OG. Coring bit can be about the same size as the pipe O.D., thus minimal sealing issue and no damage to Gunite. Ingenuity is correct....Gunite is a proprietary form of shotcrete. Concrete repair methods, if necessary, apply.
 