I need to TIG weld SA 213 T22 (P5 Gr 1) to 304 (P8) s/s plate.
Which TIG wire should I use?
E309 /AWS A5.28:ER 90SG
 
Replies continue below

Recommended for you

You should use Inconel 82 for this material combination.
 
hi-jack; in addition to mrfailure's excellent post, does anyone know of any other
standard/technical report that may give guidance for filler metal selection,
except the obvious choice of manufacturer books likes the one from Lincoln which may tell which
materials are to be welded with a certain rod/core/wire?
 
mrfailure:

where were you able to find a source for Inco Weld A Tig wire?
 