Can anyone point me to a table that gives weights of different thickness CMU walls with various cells grouted (8" oc, 16" oc, 24" oc, 32" oc, etc.)?
 
Also, I find a lot of helpful information at , the National Concrete Masonry Association. Select your state, then choose a supplier, and do a keyword search through the TEK reports.
 
Thanks guys!
 
I typically use properties found in NCMA TEK 14-1A (issued 2003). It breaks down the properties for both Average cross-section (stiffness) and Net cross-section (stress calculations).
 
It's also covered in ASCE7-02 Table C3.1 "Minimum Design Dead Loads"
 