1
- #1
I have problem with practical using of Finite Element Method in header analysis. I would like to use Gross Plastic Deformation (GPD). In this case linear elastic - perfectly plastic material model should be used. Then criterion of failure is 5% plastic strain. Unfortunately I cannot use perfectly plastic material because of problem with convergence. Insted of that I used material with tangent modulus 500MPa. After that I have no problem with convergence. I am thinking whether computed plastic strain (for material with tangent modulus) can be used to check GPD criterion (plastic strain should be less than 5%). What will be difference between computed plastic strain for perfectly plastic material and for material with tangent modulus?