Greetings,
A high tolerance sleeve with a pin that runs in it, the ID is approx 170mm with H7 fit i.e. + 40um, - 0. The sleeve finish is Good/ smooth. Good quality nitridable steel.
Can one go to final size and then gas nitride? Or I imagine ones should leave a grinding/ polishing allowance, but how much per side (or how much on internal diameter)?
Recommendations appreciated.
thx.
A high tolerance sleeve with a pin that runs in it, the ID is approx 170mm with H7 fit i.e. + 40um, - 0. The sleeve finish is Good/ smooth. Good quality nitridable steel.
Can one go to final size and then gas nitride? Or I imagine ones should leave a grinding/ polishing allowance, but how much per side (or how much on internal diameter)?
Recommendations appreciated.
thx.