Could anyone tell me where I could find this graph which shows the order of oxidation of elements in a copper bath in the 2000 - 2400 F range. I seem to remember seeing the temperature on the x axis.

Thanks
 
It sounds like you are interested in an Ellingham Diagram, do an Internet search for that.
 