Grain orientation at the hardening steel sheet

Maybe you know which is best grain orientation in hardening(quenching) so that the pieces will deform as little as possible? Transverse or rolling direction?
 
Dear barboric,

It is the rolling direction.

Regards.

DHURJATI SEN
Kolkata, India

 