Having some excessive wear issues with some of the brushes on our DC products. Anyone out there with any good info re: how to diagnose and correct the root causes of excessive brush wear in fractional HP DC motors?
 
Helwig Brushes ar in Milwaukee and are VERY good at this type of problem.
 