We are welding an offshore pipeline with Auto-GMAW process using copper shoes for backing during root pass.
We have a problem with root pass that ocurs like concavity spot 5 mm in dia. In front and after fault weld is completely sound. What could be the reason for such kind of fault? Is it some kind of impurity or discontinuity, but which one?
Welders said that they feel it like sudden suck up. We checked magnetism and it is in the expected range lower then 20 Gauss. Welding data:
Base material: X60
WT 16 mm
Gas: 100% CO2 for the root pass, 35 l/min
Wire: Autrod 12.66 dia 1.0
(270-310A and 28-30V, v=85 cm/min )
Bevel: U with nose 1.5 mm and 60 deg 1.4 mm opening from the back.
We have a problem with root pass that ocurs like concavity spot 5 mm in dia. In front and after fault weld is completely sound. What could be the reason for such kind of fault? Is it some kind of impurity or discontinuity, but which one?
Welders said that they feel it like sudden suck up. We checked magnetism and it is in the expected range lower then 20 Gauss. Welding data:
Base material: X60
WT 16 mm
Gas: 100% CO2 for the root pass, 35 l/min
Wire: Autrod 12.66 dia 1.0
(270-310A and 28-30V, v=85 cm/min )
Bevel: U with nose 1.5 mm and 60 deg 1.4 mm opening from the back.