Thank you for the reference. I've both read and posted to that thread.
The problem that exists today is that the 3M 5230 glue which was used in the testing and listed in the IBCO reports, is no longer available. Also when I checked with 3M they indicated they did not have another product equivalent to the 5230.
I know some people have used Miracle adhesive available through Tectum. I was just trying to find out if any one was using other adhesives.