May 5, 2003 #1 JerryOB Chemical Joined May 5, 2003 Messages 1 Location GB I've tried epoxy with roughening surfaces but have not had success - after a timer they come apart. Any suggestions? Jerry OB
I've tried epoxy with roughening surfaces but have not had success - after a timer they come apart. Any suggestions? Jerry OB
May 5, 2003 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US I would try a cyanoacrylate adhesive from Loctite. The following link is to their Design Guide for Bonding Plastics: http://www.loctite.com/literature/design_plastic.html Upvote 0 Downvote
I would try a cyanoacrylate adhesive from Loctite. The following link is to their Design Guide for Bonding Plastics: http://www.loctite.com/literature/design_plastic.html
May 20, 2003 #3 patprimmer New member Joined Nov 1, 2002 Messages 13,816 Location US Try 3M They make some amazing double sided tapes that give good bond strength to low surface energy plastics like PP, PE and PET. Surface preperation has to be impecable though Regards pat Upvote 0 Downvote
Try 3M They make some amazing double sided tapes that give good bond strength to low surface energy plastics like PP, PE and PET. Surface preperation has to be impecable though Regards pat