I've tried epoxy with roughening surfaces but have not had success - after a timer they come apart. Any suggestions?
Jerry OB
 
Replies continue below

Recommended for you

Try 3M
They make some amazing double sided tapes that give good bond strength to low surface energy plastics like PP, PE and PET.
Surface preperation has to be impecable though

Regards