Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Glass design building code

Status
Not open for further replies.

tdawgye

Structural
Mar 19, 2020
18
Hi there,

Are there any local building codes or standards that outline the requirements for structural glass design. Preferably Canadian code or standard.

Thank you.
 
Replies continue below

Recommended for you

What are you building? There are some standards of practice for glass guardrails and things. General glazing structural design is a bit more of a black art, but I think I have a list of references somewhere. I think there's some reasonable stuff out there for curtain walls. If it's something other than that, you're starting to get into uncharted territory a bit.

Some starting points for standards include:

EGBC Practice Guideline: Designing Guards for Building Projects
ASTM E1300
CAN/CGSB-12.20-M89 Structural Design of Glass for Buildings (Withdrawn but still referenced)
CSA A500

It had looked like CGSB-12.20 was dead, but there's a revision in progress now.

I have literally never done glass design, though. I just look at it occasionally and then decide it's not worth the hassle.
 