I am reviewing some prints for helical and spiral bevel gears that my company purchases. Under "Heat Treat" the prints state "Harden Teeth to 80-83 RA" The only Ra I am familiar with is Roughness Average. Does anyone know what RA is under heat treatment?

Thanks
 
Yes, they are carburized gears. Looks like I should review my hardness tests. Thanks!
 
If the print calls for Ra don't measure using Rc and convert as you stand the chance of punching through the case on the gear.
In your case the hardness readings will convert but the procedures will not.
It is always good practice if possible to use a method for the hardness as specified on the print and not convert.
 