Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Gap graded concrete 1

Status
Not open for further replies.

killswitchengage

Geotechnical
Jan 5, 2015
364
Hi
What are your comments on gap graded grading in regards to concrete properties especially small sized gravel from 4 to 8 mm ? i believe it can decrease the strength since it decreases the density of the concrete and it can increase the risk of shrinkage
 
Replies continue below

Recommended for you

there is a direct relationship between the amount of cement and the strength of the concrete. Beyond the minimum amount of water required for hydration of the cement, additional water does not increase strength, it reduces it.
 
kse...for a properly prepared mix design, gap grading is common. The combination of gradations and quantities are somewhat self compensating. The compressive strength of concrete is mostly controlled by the water-cement ratio. Yes, the gradation and aggregate type/source have some effect, but mostly the water-cement ratio controls. The lower the w-c ratio, the higher the strength (Abrams law).

As for the smaller aggregate size....when you reduce the coarse aggregate size, the cement content has to be increased because the surface area of the aggregate must be coated with cement paste for adequate bond. Smaller coarse aggregate particles have a higher specific surface than larger coarse aggregate.
 
See Neville's tome on gap grading of aggregate for background.
 