Gregorydas
Mechanical
Hi all,
This question has evolved during the fabrication of 100 No's of sliding gate. Client need a guarantee of 5 Years for the corrosion. We are giving a 3 coat paint system and the paint manufacturer gives 2 year warranty on the paint. They also recommended galvanizing or electroplating before the application of the paint. The gates are to be installed on corrosive environment (SALTY AIR - BAHRAIN PORT AREA)
So I am a bit confused regarding the selection. What is the common difference between Galvanizing and Electroplating? Which would be costlier? and which would give a sufficient corrosion protection for 5 years, along with the application of 3 coat paint system (225 Microns - Epoxy Primer, Mastic Coat and Polyurethane top coat for gloss)
The gate is 4.4 Wide and 2.5 m high. With Hollow section Frame and Square bar designs + Poly carbonate Sheet and a small design made of 1.5 mm GI Sheet.
This question has evolved during the fabrication of 100 No's of sliding gate. Client need a guarantee of 5 Years for the corrosion. We are giving a 3 coat paint system and the paint manufacturer gives 2 year warranty on the paint. They also recommended galvanizing or electroplating before the application of the paint. The gates are to be installed on corrosive environment (SALTY AIR - BAHRAIN PORT AREA)
So I am a bit confused regarding the selection. What is the common difference between Galvanizing and Electroplating? Which would be costlier? and which would give a sufficient corrosion protection for 5 years, along with the application of 3 coat paint system (225 Microns - Epoxy Primer, Mastic Coat and Polyurethane top coat for gloss)
The gate is 4.4 Wide and 2.5 m high. With Hollow section Frame and Square bar designs + Poly carbonate Sheet and a small design made of 1.5 mm GI Sheet.