Dec 1, 2012 #1 ENPMAT Materials Joined Jun 27, 2012 Messages 9 Location DZ Dear All, I know that SS are better than HDG Steels. But when we HDG steels can be used instead of SS, and when this substitution is no acceptable. Is there any standard or common practice specially in oil and gas industry. Thanks.
Dear All, I know that SS are better than HDG Steels. But when we HDG steels can be used instead of SS, and when this substitution is no acceptable. Is there any standard or common practice specially in oil and gas industry. Thanks.
Dec 2, 2012 #2 cloa Petroleum Joined Jul 18, 2008 Messages 1,071 Location JP Not true at all. Stainless Steels are different. 304 is worse than HDG in certain offshore platform applications due high propensity to pit. Upvote 0 Downvote
Not true at all. Stainless Steels are different. 304 is worse than HDG in certain offshore platform applications due high propensity to pit.
Dec 12, 2012 #3 TonyDeRamo Structural Joined Nov 15, 2011 Messages 11 Location US One must also consider venting for HDG. If vent holes are unacceptable in a certain application then the use of HDG is not an option. "Research is what I'm doing when I don't know what I'm doing." Upvote 0 Downvote
One must also consider venting for HDG. If vent holes are unacceptable in a certain application then the use of HDG is not an option. "Research is what I'm doing when I don't know what I'm doing."