Hello All
Background:
The specification states that the Weld shall not be Anodic with respect to Base material, This statement appears as the acceptance criteria under Galvanic Corrosion Test of the Pipe Procurement specification.
Suppose the potential measured of the pipe base material is "- 0.5" and the potential of the weld is "-0.4" (I persume it is the potential that will be determined as the measure of Anodicity or Cathodicity), is the Weld Anodic with respect to Pipe.
Background:
The specification states that the Weld shall not be Anodic with respect to Base material, This statement appears as the acceptance criteria under Galvanic Corrosion Test of the Pipe Procurement specification.
Suppose the potential measured of the pipe base material is "- 0.5" and the potential of the weld is "-0.4" (I persume it is the potential that will be determined as the measure of Anodicity or Cathodicity), is the Weld Anodic with respect to Pipe.