UMDpru
Mechanical
- May 16, 2007
- 41
I have been asked to review the corrosion potential of a bolted joint. The fastener material is MP35N. This fastener is being used to bolt together two pieces of Monel K-500. The environment will be in seawater and the flow rates around the fastener head are likely to be very very low if any at all.
I have been reading a great deal and have come to the conclusion that MP35N is susceptible to Galvanic corrosion when used in the preceeding fassion. The question for me now is how much corrosion can I expect and over what time frame.
I am primarily a Mechanical Engineer and I have no background in Corrosion Engineering so I was wondering if someone more experienced could provide some insight or direction...
My Mechanical group really has no one experienced with corrosion either so I am alone with this.
any help would be appreciated...