The link below suggests that there can be a severe galvanic corrosion risk when magnesium is adjacent to stainless steel.


My question is if this is true, does that mean that you should not use a steel or stainless helical insert (helicoil) or staked-in insert such as a keensert in a part made of magnesium? It is standard practice for my group to use stainless inserts when we design similar components using aluminum.

Kilkenny
 
Replies continue below

Recommended for you

For tools and fixtures, used in ambient-temp., dry environments, we used Keenserts (generally steel, but also stainless) and never had trouble. That said, I'd think hard if the aluminum or magnesium part were to be used in moist or marine environments, as the posts last week have pointed out.
 
Whoops -- See the posts regarding inserts in aluminum parts in the corrosion engineering section.
 
Yes, it is true that severe galvanic attack will occur if magnesium and stainless steel are connected in the presence of an electrolyte. You will need to use other materials or coatings to eliminate this problem.