Galvanic Corrosion : Inconel 625 x 309SS 1

Status
Not open for further replies.

ibf

Mining
Feb 25, 2004
83
How far apart are they on the Galvanic chart ? Would Galvanic corrosion be a potential risk between them ?

Thank you.



 
Replies continue below

Recommended for you

What is the environment?

In neutral pH environments there won't be much potential diff.
If you are in high Cl or lower pH then the 309 will see accelerated failure, but it wouldn't work well there anyway.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 