Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Galvanic Corrosion Between Inco 625 and K500 1

Status
Not open for further replies.

FastenerDude

Industrial
Joined
Jan 3, 2013
Messages
17
Location
GB
Will galvanic corrosion occur between Inco 625 and K500 material? I have a customer who wants to buy a Inco 625 Socket Head Cap Screw along with a K500 lockwasher. The environment will be subsea. I offered a K500 lockwasher b/c you can get a "true" lockwasher in this material where as with Inco 625, you are basically getting a flat washer that is split.

Greg
System 22, Inc.
 
What are they screwed into?
If it is less corrosion resistant then either then there is no issue.
I doubt that there will be problems, though in the past I strongly favored using K500 for washer and bolt.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
The screws will be installed into a fabricated part made completely out of Inconel 625.

Greg
System 22, Inc.
 
If the parts receive cathodic protection, the issue goes away.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 