OSUCivlEng
Civil/Environmental
The client wants to do full pen welds for bearing stiffeners on a plate girder instead of mill to bear with fillet welds. My understanding is fabricators don't like it because it causes distortion to the flanges. It also adds NDT testing cost and is a more expensive weld. I would tend to agree since there are 40 stiffeners times 2 welds (top and bottom) for a total of 80 full pen welds.
The client says full pen welding provides better bearing and there shouldn't be any distortion with 1" thick flanges. I am not sure how he arrives at his conclusions.
This would seem to confirm my thoughts as well.
I am curious what other engineer's experiences are?
Thanks
The client says full pen welding provides better bearing and there shouldn't be any distortion with 1" thick flanges. I am not sure how he arrives at his conclusions.
This would seem to confirm my thoughts as well.
I am curious what other engineer's experiences are?
Thanks