Im trying to make a part of which common pourable RTV silicone is ideal as it needs to be cast. Only problem is it must be reasonably fuel (gasoline) resistant which all RTV's I've tried are not.
It's doesn't need to be silicone. Any rubber about 30 Shore hardness will do.
Thanks.
It's doesn't need to be silicone. Any rubber about 30 Shore hardness will do.